Discussion:
Ceramicrete
(too old to reply)
jaco
2007-09-21 20:04:14 UTC
Permalink
Hi, anyone have any news on ceramicrete ? where can you buy this
material ? what are people doing or planning with this material ?
Gregg
2007-09-21 22:05:44 UTC
Permalink
Post by jaco
Hi, anyone have any news on ceramicrete ? where can you buy this
material ? what are people doing or planning with this material ?
Sounds like an extension of phosphate cement and phosphate bonding used
in the refractories industry.
I've seen or used similar chemistry for enhancing phosphate bonded cores
and refractories.

http://www.anl.gov/techtransfer/Available_Technologies/Material_Science/Ceramicrete/index.html

The above links has contact information as well as patents.
The technology transfer office should be willing to provide help for a
particular application.
When I checked into ORNL's gel casting technology, they asked me to come
to ORNL for several days. I was able to work with the principle
inventor while they performed a series of trials with our ceramic
composition.
Can't ask for better service than that!

Argonne might do the same.

Gregg